D001 SC macroporous cation exchange resin is a polystyrene matrix, macroporous strongly acidic cation exchange resin. containing sulfonic acid, solid sulfate, equivalent.Uniform pore size, high mechanical strength. Mainly used for high-speed mixed bed water treatment.
Index
Name |
Specification |
Appearance |
White to light yellow opaque spherical beads. |
Polymer |
Styrene-DVB-Copolymer, Macroporous |
Functional Group |
Sufluric Acid |
Ionic Form |
Na+ |
Weight Exchange Capacity |
≥4.35mmol/g |
Volume Exchange Capacity |
≥1.8mmol/ml |
Real Density (g/ml) |
1.25~1.28g/ml |
Bulk Density (g/ml) |
0.77~0.85g/ml |
Water Retention Capacity |
45%~55% |
Particle Size Range |
0.63~1.25 mm≥95 |
Uniformity Coefficient |
≤1.4 |
Whole Bead Count(%) |
≥95% |
Reference Operation Conditions
Maximum operating temperature |
120℃ |
Resin filling height |
1~3m |
Operating velocity |
2~10BV/h |
Backwash velocity |
4~10BV/h |
Regeneration (desorption) velocity |
1~2BV/h |
Regeneration agent |
2BV3~5%HCI,2BV2~4% NaOH |
Application
High-speed mixed bed water treatment
Recycling of precious metals
Organic catalysis
Corresponding Brands
Amberlite 200
Lewatit Sp-210
Purolite C150
Precautions
Resin should be wet state preservation. The best temperature is above 0℃. Resin should be put into a closed space or add in salt water of 5% or above if not used for a long time.Should be anti-freezing during transportation. Do not place heavy objects on the resin in case being crashed.
Generally requires alkali- water - acid - water flow path for processing. Strict requirement needs three circulation before coming to final ion kenel.
Need to consider different transformation expansion rate to set aside enough space to prevent resin overflow and ensure the appropriate liquid level height; Column diameter ratio should be within a reasonable range and avoid bias current; Use wet packed column or back-flushing to wash away bubbles inside resin layer.
Before liquid going into the resin column, steps as flocculation, filtration, or sand-filtration should be taken so that it doesn’t jam resin pore with suspended solids .